Before applying interior films, the surface condition of where to be applied must be checked for a proper installation.
MDF
- Apply a sufficient primer to the surface of substrate (MDF, PB, etc.) 1-2 times.
- Since the cutting (slit) surface of wood has a high absorption rate and uneven surfaces, the primer should be fully applied 2-3 times.
- Primers will need approximately 2 hours drying time. It is advised and recommended that you check the substrate and thoroughly dry and clean prior to installation.
- Once the primer surface is dry enough, make the surface smooth and overlappping section is needed to be cleaned with sandpaper and remove residue with a lint free cloth and make sure area is completely dust free.
- Color differences may occur between product lots, so you must confirm the color with the pre-attached product before purchasing.
- Surface treatment by using sandpapers is required and make sure the surface is clean before applying primer to enhance adhesion performance.
- Please make a pressure using by Helt or Hera (Spatula). Rubbing or Hard Pressure may work to stengthen the Adhesion 2 -3 times.
- Apply interior films carefully, not wrapping films forcefully pull over MDF plates, heat or humidity can cause a MDF distortion.
SC/SE (man-made leather type)
- Do not overlap due to the embossed depth and please apply Solvent Type Primer to press firmly.
- In order to maximize the visual effect of the product, it is necessary to check the type and condition of the surfaces and remove all residues prior to installation. Do not rub too hard.
SP
To enlarge the design effect, the film is too soft on the top. Please do not rub too hard.
JG/JF
JG/JF is specially processed using Alumium, detachment of where film lines are overlapped can cause a peeling of films surfaces. So pay attention at installing
PREMIUM MATT LINE-UPs, SOFT MATT (Soild)
- As being treated with a special process on the surfaces, it feels initially not sticky enough in the overlapped parts, but being fully pressed adhesive parts will be stabilized stronger over time. (Method when contaminated : Wipe with an alkaline alcohol to remove.)
- Please avoid moisture and direct sunlight, and please do not use it outdoors.
- The surface may become discolored during prolonged exposure to sunlight or ultraviolet light.
- It is recommended that correct storage temperatures are used for storing the product to be free from long term storage defects.
(15°C to 25°C)
- When installing the film, please use manufacturer’s recommend products.